PET bottle appears pearl gloss white

Reasons: 1, the heating temperature is too low 2, the thickness of the germ tube wall is 3, the thickness of the embryo tube is too thick, and the temperature is not enough.

Exclusion method: 1, heating or slow speed of revolution 2, to improve the embryo quality 3, reduce germ tube thickness, or to attempt to raise heating device housing, to increase the germ tube surface temperature distribution


On service:Position offset of bottom nozzle of PET bottle